The Performance Qualification (PQ) carried out as part of the initial validation and for re-validation requires determination of the seam strength. Seal samples can be created precisely at the required width of 15 mm using sample cutters. These are then clamped into the testing machine or adaptive testing device and peeled at a monitored speed of 200 mm/min. The strength curve and maximum strength are recorded. Clamp kit for blister packs on request.
The software for tensile strength testing has been completely revised and from 2019 also meets the requirements of the new EN 868-5:2019.
Catalogue No | Description | Unit |
---|---|---|
0.617.293 | ht 150 SCD:2019 | 1 pcs |